Bar Molding Defect

Alan B
@alan-b
02/10/13 12:30:19
7 posts

Thank you very much for the suggestions. My room is at around 68 F, but I did neglect to warm the molds prior to filling them :( I wasn't sure what this defect was called--thank you for explaining that this is a release mark.

Best wishes,

Alan

Chocotoymaker
@chocotoymaker
02/09/13 17:02:40
55 posts

Either your room or your molds are too cold when you pour your chocolate. Plus there is no need to wait a few hours before de-moulding.

Take a hair dryer and heat the molds with it for about 3 seconds that should take care of your release marks. Leave them in the fridge as long as needed for them to completely release and then just take them out without letting them sit for hours.

Alan B
@alan-b
02/06/13 21:17:52
7 posts

I am new to The Chocolate Life and would appreciate the group's thoughts on this recurrent problem I'm having with bar molds. I have attached a couple of pictures of recent snafus. After filling my well-cleaned polycarbonate molds with precystallized dark chocolate (from Guittard), I place them in the refrigerator for around 10-15 minute and then place the molds at room temperature for a few hours before releasing the bars. As the photosDSCF1724.JPGandDSCF1729.JPGshow, there are dull spots on the bars and corresponding thin amounts of chocolate on the mold. The locations of these defects changes with subsequent moldings. This leads me to think this is not due to a defect in the polycarbonate mold, but rather a problem with how the chocolate is setting up. The chocolate that I am using appears to be properly precrystallized. I'm wondering if refrigeration could be playing a role?

I would appreciate any thoughts on the cause of this problem and possible solutions.

Thanks, in advance, for your advice.

Alan B


updated by @alan-b: 04/11/25 09:27:36

Tags

Marketplace

Activity

kapil jain
 
kapil jain
 
kapil jain
 
@kapil-jain • 9 years ago

Chocolatevenue is an online chocolate store in India.We are specialized in customized chocolates .Chocolates can be customized as chocolate message and chocolate bars.

You can get written your message on chocolates and can get customized your chocolate bars by selecting the desired ingredients.

for more details

https://www.chocolatevenue.com 

colorchocolate
 
@colorchocolate • 9 years ago

FOR SALE / BARGAIN / FINE CACAO LIQUOR, COLOMBIA ORIGIN

Enjoy a delicious premium chocolate from the Boyacá region of Colombia, considered among the best in the world. We offer a 200 kilograms lot of pure origin cocoa liquor,  fair trade / ethically sourced. No other ingredients added.

The price for this high quality product is as follows:

1 kg - US$ 13

100 kg - US$ 12 per kilo

200 kg - US$ 11 per kilo

Inquires: equalcolombia@gmail.com

- See more at: https://www.thechocolatelife.com/colorchocolate#sthash.JFDWYFuK.dpuf

- See more at: https://www.thechocolatelife.com/community/forums/my_posts/18453/fine-cacao-liquor-colombia-origin#sthash.2pUq4Eu3.dpuf

Clay Gordon
 
@clay • 9 years ago

FCIA Recognition of Excellence Nominations close in one week: https://fcia.wufoo.com/forms/r1lzjl7w1w9ri8n/

Clay Gordon
 
The 4 Chocolatiers
 
@the-4-chocolatiers • 9 years ago

Two changes we made with the chocolate is that this time we winnowed the chocolate. This time we didn't use a blow dryer to melt the chocolate. Two improvements with the chocolate is that the melanger didn't get clogged this time and everyone put in work.